Mechanical seal after long-term operation, the end face of the moving ring and the static ring due to friction wear, spring and sleeve will also occur rust or damage, the sealing ring due to aging deformation and lose elasticity, all these reasons will cause mechanical seal leakage.
Therefore, after a long period of operation, the mechanical seal components should be replaced or repaired to achieve the purpose of reuse.
(1) Grinding of end faces of moving rings and static rings.
After the moving ring is removed, the grinding process is carried out, first rough grinding, then fine grinding, and then polishing when conditions are available.
Coarse grinding, the selection of 80~160 particle size of abrasive, grinding to the processing trace first.
Then can use more than 160 abrasive for fine grinding, so that the finish to meet the design requirements, hard alloy or ceramic moving ring fine grinding after the need to use polishing machine polishing.
The strength of polishing machine can choose M28~M5 boron carbide.
Polished to a mirror surface.
The ceramic ring can be finely ground with M5 agate powder and polished with chromium oxide.
Graphite filled ptfe static ring, because the material is soft, can be refined by kerosene, gasoline or water, do not need to add abrasive.
In the process of running together can also be self-research, so the requirement of finish is not too high.
The method of grinding, with a grinding machine can be ground in the grinding machine, no grinding machine can be used in the plate glass figure 8 manual grinding method.
(2) Sleeve inspection.
After the overhaul and removal of the shaft sleeve, check the corrosion and wear. If the corrosion or wear is relatively slight, fine sandpaper can be polished and reused. If the corrosion or wear is serious, the method of electroplating after processing can be used or a new shaft sleeve can be replaced.
(3) Sealing ring.
After a period of time, the sealing ring loses elasticity or aging in most cases, and generally needs to be replaced with a new ring.
(4) spring.
If the spring corrosion is not serious, can keep the original elasticity, can not be replaced.
If the rust is more serious or elasticity is reduced a lot, you need to replace the new spring.
For mechanical seals with assembled boxes, the boxes should be cleaned and the grooves checked for wear or deformation for correction, regrooving or replacement.
After repairing the mechanical seal elements, they are reassembled and subjected to the same pressure test before being put into normal operation.